MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Ulti-Plex® Synthetic Grease EP
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Features

Chevron Ulti-Plex Synthetic Grease EP is a multipurpose, high performance grease specially formulated for extreme pressure bearing applications operating under the most extreme high and low temperature conditions and for those difficult applications requiring extended lubrication intervals.

It is manufactured using selected highly refined high viscosity synthetic base oils, a lithium complex thickener, rust and oxidation inhibitors, and extreme pressure and tackiness additives. It is light tan in color and smooth and buttery in texture.

Chevron Ulti-Plex Synthetic Grease EP provides an alternative for high temperature applications. The uniform molecular structure of the synthetic base oils minimizes friction between moving parts and boosts lubrication performance over a wide temperature range.

The high viscosity index of the synthetic base oils allow for greater pumpability at subzero (-29°C/-20°F) temperatures, allowing bearings lubricated with Chevron Ulti-Plex Synthetic Grease EP to operate at temperatures as low as -51°C (-60°F).

Applications

Chevron Ulti-Plex Synthetic Grease EP is recommended for use in applications with temperatures up to 232°C (450°F), with a dropping point of approximately 288°C (550°F).

Chevron Ulti-Plex Synthetic Grease EP is ideal for a wide variety of applications across several industries, including:

  • Paper and Forest Products — This lubricant is superior for severe service applications such as: sludge press bearings, lime kilns, pumps, woodyard heavy equipment, Doctor oscillator bearings, felt roll bearings, pulp refiner bearings, rope sheaves, and exhaust fan bearings. Chevron Ulti-Plex Synthetic Grease EP is particularly well-suited for the highest temperature applications, such as felt roll bearings and lime kilns operating at temperatures in excess of 204°C (400°F).
  • Mining — Chevron Ulti-Plex Synthetic Grease EP is particularly recommended for
    • mining operations that involve extreme pressure applications requiring excellent low temperature pumpability. Applications include: pins and bushings on buckets and loaders, shaker screens, crushers, and conveyors
    • the lowest temperature mining applications
    • automatic lubricating systems in onboard shovels, trucks, and other mobile equipment
  • Off-Road Construction — This grease is ideally suited for lubrication systems that involve pumping grease through long supply lines at low temperatures. It also displays superior water washout resistance properties in wet, off-road environments.
  • Steel — Steel mill applications often involve extremely high temperatures. The excellent structural stability of Chevron Ulti-Plex Synthetic Grease EP makes it appropriate in these situations. Its extreme pressure properties and superior resistance to water washout are also key in the steel mill environment. This grease provides outstanding protection for steel mill roll bearings, conveyors, furnace and coiler grease points, pump bearings, and exhaust fan bearings.
  • Marine — The rust and corrosion inhibition properties of Chevron Ulti-Plex Synthetic Grease EP make it ideal for use in marine equipment exposed to severe corrosion environments. Examples include deck equipment, offshore drilling equipment, grease lubricated shaft bearings, cranes, and windlass winches.
Chevron Ulti-Plex Synthetic Grease EP is approved for NLGI Certification Mark LB.

Chevron Ulti-Plex Synthetic Grease EP is registered with NSF and is acceptable as a lubricant where there is no possibility of food

Key Words: CPS Number: 250188; MSDS Number: 5343
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 148Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1791 SUS
Saybolt Viscosity at 210°F 172 SUS
Kinematic Viscosity at 40°C (104°F) 344 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 35.5 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 500 kgWeld Point
Four Ball Wear 0.260 mm
Penetration 315Worked
Penetration P(0), 1/10 mm 295
Timken Test 50.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 235 °C
Minimum Service Temperature, Air -51.0 °C
Flash Point 280 °CASTM D92
Dropping Point 312 °C
 
Descriptive Properties
Bearing Water Washout wt% Loss at 175°F5 wt% loss at 175°F
ColorLight Tan
Corrosion, Copper Strip Test 3h1B
Lincoln Ventmeter, psig at 30 s, at 0°F517
Lincoln Ventmeter, psig at 30 s, at -22°F725
Lincoln Ventmeter, psig at 30 s, at 75°F38
TextureSmooth, Buttery
Thickener, % / type13 / Lithium Complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Ulti-Plex® NLGI 0 Greases EP

WCHEV278 / 74893

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.