Medium molecular weight, medium density film resin Characteristics: - Excellent balance of stiffness and impact strength
- Good puncture resistance
- Excellent compatibility with LDPE and LLDPE
- Good tensile strength
- Good heat sealing characteristics
Applications: - Specialty Merchandise bags
- Mailing envelopes
- Heavy-duty shipping sacks
- Pallet shrink films
- Fresh cut produce packaging
- Coextrusion
This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture. |
Excellent balance of stiffness and impact strength |