Base Polymer: Polycarbonate Filler/Additive System: Special filler, halogen-free flame retardant, UV stabilized Special Features: Light scattering, high light diffusion, good flow, processing stabilized, injection molding grade Market Segment: Automotive, Lighting, Electrical and Electronic Typical Application: Lamp covers, display elements, operating elements Information provided by Albis Plastics |