- Extrusion- and injection molding grade
- very good hydrolysis and microbial resistance
- good low-temperature flexibility
- complies with VDE 0282-10
- very large processing window
Application- Cable sheathings
- Hoses
- non-reinforced
- Profiles
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |