MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® H525 High Density Polyethylene, Pressure Pipe Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: This high performance PE 4710 HDPE is tailored for demanding pressure pipe applications that require:
  • Good long-term hoop strength
  • Good resistance to slow crack growth
  • Excellent resistance to slump

Additional Information

  • Meets ASTM D4796 - PE 235

Typical applications for H525 include:

  • Municipal, industrial and mining pipe
  • Oil and gas-gathering pipe

When blended with an approved black concentrate, the material meets or exceeds:

  • ASTM D3350, cell classes 445574C
  • NSF Standards 14 and 61 for potable water
  • PPI designations PE 4710

Information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.948 g/ccASTM D1505
Melt Flow 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 500 hourASTM F1473
Tensile Strength, Yield >= 24.0 MPa2 in/min, Type IV bar; ASTM D638
Elongation at Break >= 700 %2 in/min, Type IV bar; ASTM D638
Flexural Modulus 830 MPa
@Strain 2 %
Secant; ASTM D790
Hydrostatic Design Basis 6.90 MPa
@Temperature 60.0 °C
ASTM D2837
 11.0 MPa
@Temperature 23.0 °C
ASTM D2837

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin
Chevron Phillips Marlex® H516HP High Density Polyethylene, Pressure Pipe Grade
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
Chevron Phillips Marlex® HP132 High Density Polyethylene, Pressure Pipe Grade
Chevron Phillips Marlex® HMN 6060 Polyethylene, Injection Molding Grade, HDPE

PCHEVC916 / 130399

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.