MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 502XT PA6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Description: Unreinforced polyamide 6, very high viscosity, for extrusion.

Available in: Europe

Product Applications: It is suitable for extruded semi-finished products, such as: Rods, profiles, sheets, pipes. All the semi-finished products can be machined without special treatment, such as: Precision gears, bolts, etc. This product is available in natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183/A
Water Absorption 1.37 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 80.0 MPaISO 527 type 1 A
Elongation at Break 160 %ISO 527 Type 1A
Elongation at Yield 4.2 %ISO 527 type 1 A
Tensile Modulus 2800 MPaISO 527 Type 1A
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180/1eA
Charpy Impact Unnotched NBISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 3.4IEC 60250
Dielectric Strength 22.0 kV/mmIEC 60243
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CISO 11357
 
Processing PropertiesOriginal ValueComments
Feed Temperature 230 °C
Front Barrel Temperature 230 °C
Die Temperature 240 °C
 
Descriptive Properties
Compression Zone230ºC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® C 536XT PA6, DRY
Covestro Makrolon® ET3117 Polycarbonate
Overview of materials for Nylon 6, Extruded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
NYCOA 578 PA 6

PRHOD810 / 138041

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.