System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Inno-Comp INNOPOL® CS 5-8250 W 50% Chalk-Filled High Density Polyethylene
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 50% Calcium Carbonate
;
Polypropylene, Film Grade
Material Notes:
INNOPOL® CS 5-8250 W is a 50% chalk-filled compound based on high density polyethylene.
INNOPOL® CS 5-8250 W is developed for packaging film production.
All information provided by INNO-COMP.
Key Words:
HDPE
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.46
g/cc
@Temperature 23.0 °C
ISO 1183
Melt Flow
0.35
g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Film Elongation at Break, MD
>= 250 %
ISO 527
Film Elongation at Break, TD
>= 100 %
ISO 527
Elmendorf Tear Strength MD
12
g
ISO 6383-2
Elmendorf Tear Strength TD
140
g
ISO 6383-2
Dart Drop Test
20.0
g
ISO 7765
Film Tensile Strength at Break, MD
15.0
MPa
ISO 527
Film Tensile Strength at Break, TD
8.00
MPa
ISO 527
Descriptive Properties
Color
White
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
LG Chemical SEETEC PH150 HDPE Blown Film Grade
Kraton® D1102 + HDPE blend (10/90)
Kazanorgsintez PE2NT 11-285 High Density Polyethylene Composite
Ipiranga Petrochem GM 9450 F HDPE
PINNO067 / 82728
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.