MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haysite H900 Polyester, Glass Reinforced
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: H900 is recognized throughout the world as a reliable, consistent GPO-3 material. Standard size sheets are available in thicknesses ranging from .094" to 2.00". H900 also exhibits excellent smoke, flame and toxicity characteristics. Govt. Spec I-24768/6. Standard color - red.

Information provided by Haysite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/ccASTM D792
Water Absorption 0.20 %ASTM D229
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 62
Tensile Strength 9000 psiASTM D638
Flexural Strength 18000 psiASTM D790
Flexural Modulus 1.50e+6 psiASTM D790
Compressive Strength 30000 psiASTM D695
Shear Strength 14000 psiASTM D732
Adhesive Bond Strength 1400 psi
@Thickness 12.7 mm
ASTM D229
Izod Impact, Notched 8.00 ft-lb/inEdgewise; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength 450 V/milPerpendicular, short time in oil; ASTM D149
Dielectric Breakdown 55000 VParallel, Step-By-Step in Oil; ASTM D149
Dissipation Factor 0.060
@Frequency 60 Hz
ASTM D150
Arc Resistance 190 secASTM D495
Comparative Tracking Index >= 600 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Inert 160 °C
Flammability, UL94 V-0
Smoke Density 4.0 min0.33 Optical Density; ASTM E661
 
Descriptive Properties
Flame Resistance130 secondsIgnition Time, ASTM D229
 33 secondsBurning Time, ASTM D229
Inline Plane Track Resistance1000 minsASTM D2303
Radiant Panel5ASTM E162
Tunnel Test<251/4", ASTM E84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Extruded
A. Schulman Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC
Overview of materials for Acetal Homopolymer, Unreinforced
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass
Quantum Composites QC-8777 41% Glass Fiber Reinforced Polyester Hybrid SMC

PHAY515 / 142471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.