MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman POLYPUR™ FPU 1185 Thermoplastic Polyurethane Compound
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded; Polyurethane, TP

Material Notes:
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8515 sec delay; ASTM D2240
Tensile Strength, Ultimate 34.0 MPa20 in/min, at max load; ASTM D638
Elongation at Break 500 %ASTM D412
Flexural Modulus 0.0270 GPa1.3 mm/min; ASTM D790
Tear Strength 500 pli2 in/min; ASTM D624
Compression Set 16 %
@Temperature 23.0 °C,
Time 79200 sec
Method B; ASTM D395
 65 %
@Temperature 70.0 °C,
Time 79200 sec
Method B; ASTM D395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 2786A Thermoplastic Polyurethane
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound
BASF Elastollan® 1185 A FHF TPUR Flame Retardant Halogen Free
BASF Elastollan® 1185 A W TPUR

PASHU271 / 25235

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.