MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Intene® 60 AF Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Intene® 60 AF is a solution polymerized low cis polybutadiene produced using an alkyl lithium catalyst. A TNPP/BHT free, food contact approved, non-staining antioxidant is added during the production process.

Key Features: Low cis BR is the polybutadiene of choice to produce high impact Polystyrene (HIPS). Intene® 60 AF is particularly suited to applications where environmental stress cracking properties and/or improved impact strength are required.

Main Applications: Impact improver to be used in polystyrene and ABS manufacturing.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Viscosity 250 cP
@Temperature 25.0 °C
250 cP
@Temperature 77.0 °F
of Solution, 5% wt/wt in Styrene
Ash <= 0.050 %<= 0.050 %ASTM D5667
 
Descriptive Properties
Apha Color5ASTM D1209
Cis - 1:4 Content, min38%Internal Method
Gel Rating, max5Internal Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR)
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Dow SE BCP 817 Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1203H Stereospecific high cis-1,4 Polybutadiene (BR)

PENG201 / 124595

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.