Notes: Monprene CP-18960 is a clear general purpose thermoplastic elastomer, available in NAT and BLK, designed for a variety of industrial and consumer product applications requiring a soft, rubber-like feel. Monprene CP-18960 is a medium hardness, low density, unfilled, UV resistant grade that is suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Contact Clarity; General Purpose; Good Colorability; Low Density; Low Specific Gravity; Medium Flow; Medium Hardness; Slip; Sunlight Resistant; UV Resistant; Without Fillers Uses: Consumer Applications; Flexible Grips; General Purpose; Industrial Applications; Rubber Replacement RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Preliminary data. Information provided by Teknor Apex |