MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling SUSTAMID® 12 MO PA 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product characteristics:
  • Low moisture absorption
  • High UV resistance
  • High chemical resistance
Product applications:
  • Mechanical engineering
  • Aircraft construction
  • Construction industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³DIN EN ISO 1183-1
Water Absorption 0.80 %0.80 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878DIN EN ISO 868
Tensile Strength, Yield 50.0 MPa7250 psiDIN EN ISO 527
Elongation at Break 150 %150 %DIN EN ISO 527
Modulus of Elasticity 1.80 GPa261 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²DIN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C55.6 µin/in-°FDIN 53752
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°FDIN 52612
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FDIN 52612-1
Melting Point 178 °C352 °FISO 11357-3
Maximum Service Temperature, Air 80.0 °C176 °Flong term
 140 °C284 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FDIN EN ISO 75
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 204F  Nylon 12 (PA 12) Glass Fiber 25%
RTP Company RTP 203.3F  Nylon 12 (PA 12) Glass Fiber 23%
RTP Company RTP 202F  Nylon 12 (PA 12) Glass Fiber 15%
RTP Company RTP 200F TFE 13 SI 2  Nylon 12 (PA 12) PTFE 13% - Silicone 2%
RTP Company RTP 200F MS 2  Nylon 12 (PA 12) Molybdenum Disulfide 2%

PROCH9293 / 232995

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.