MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Marco Polo MARPOL HDF 504 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: MARPOL® HDF 504 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics. MARPOL® HDF 504 is well balanced in overall physical properties and provides good stiffness for thin gauge film applications.

Recommended application: T-shirt bags, trash can liners, industrial liners, heavy bags, produce bags on a roll.

Additives: Antiblock – no, Slip – no, Thermal Stabilizer – yes.

This resin complies with FDA regulation 21 CFR 177.1520 (c) 3.1a, and may be used as articles or components of articles intended for packaging or holding food, except during cooking

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.949 g/cc0.0343 lb/in³ASTM D1505
Melt Flow 0.040 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.040 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 27.6 MPa4000 psiASTM D882
Film Tensile Strength at Yield, TD 25.5 MPa3700 psiASTM D882
Film Elongation at Break, MD 300 %300 %ASTM D882
Film Elongation at Break, TD 410 %410 %ASTM D882
Flexural Modulus, 1% Secant 862 MPa125000 psiMD; ASTM D882
 889 MPa129000 psiTD; ASTM D882
Elmendorf Tear Strength MD 12 g12 gASTM D1922
Elmendorf Tear Strength, MD 0.984 g/micron25.0 g/milASTM D1922
Film Tensile Strength at Break, MD 62.1 MPa9000 psiASTM D882
Film Tensile Strength at Break, TD 28.3 MPa4100 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C268 °FASTM D3418
 
Optical PropertiesMetricEnglishComments
Haze 29 %29 %ASTM D1003
Gloss 22 %22 %45°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO196 / 283793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.