MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 9740 Double Coated Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tape 9740 is a 3.5 mil double coated tape utilizing a 0.5 mil (12 microns) polyester film coated on both sides with 1.5 mils (38 microns) of a high shear acrylic adhesive system. This adhesive system allows for superior bonding and conformability to irregular as well as flat surfaces, and bonds well to most substrates including most low surface energy plastics. Performance grade splicing tape for corrugators and other high temperature splicing applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 12.7 microns0.500 milCarrier
 38.1 microns1.50 milTape
 38.1 microns1.50 milTape
 88.9 microns3.50 milTotal (excluding liner)
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.82172 kN/m4.6875 plito Steel, Initial, 12 in/min
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 219 °C426 °F
Minimum Service Temperature, Air -12.0 °C10.4 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Adhesive CarrierPolyester
Adhesive TypeAcrylic
AppearanceClear
Liner55# DK

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33294 / 168041

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.