MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Hifax™ CA244 Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hifax™ CA244 high melt flow, 850 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has an excellent combination of stiffness, processability and dynamic impact characteristics. It was designed primarily for use in painted automotive bumper fascia applications where material flow is an important consideration. Uses: Automotive exterior parts

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
16 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 868
Tensile Strength at Break 11.0 MPa1600 psiISO 527-1, -2
Tensile Strength, Yield 18.0 MPa2610 psiISO 527-1, -2
Elongation at Break 500 %500 %ISO 527-1, -2
Elongation at Yield 14 %14 %ISO 527-1, -2
Flexural Modulus 0.848 GPa123 ksiISO 178
Izod Impact, Notched (ISO)  3.90 kJ/m²
@Temperature -40.0 °C
1.86 ft-lb/in²
@Temperature -40.0 °F
ISO 180
 33.0 kJ/m²
@Temperature 23.0 °C
15.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Dart Drop, Total Energy 25.0 J
@Temperature -30.0 °C
18.4 ft-lb
@Temperature -22.0 °F
Instrumented; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FUnannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 47.2 °C117 °FUnannealed; ISO 75A-1, -2
Shrinkage 0.80 %0.80 %Tool, 100x150x3.2 mm; Basell Test Method
 1.1 %
@Temperature 121 °C,
Time 3600 sec
1.1 %
@Temperature 250 °F,
Time 1.00 hour
Afterbake, 100x150x3.2 mm; Basell Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hifax™ CA287AHF Thermoplastic Polyolefin Elastomer
LyondellBasell Dexflex 980 BLK Thermoplastic Polyolefin
LyondellBasell Dexflex 810 BLK Thermoplastic Polyolefin
LyondellBasell Hifax™ CA10GC Thermoplastic Polyolefin Elastomer
LyondellBasell Hifax™ CA187 Thermoplastic Olefin Resin

PMO779 / 53768

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.