MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® TSG-30/4 V0 PA666-GF30 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Product description: Grilon TSG-30/4 V0 is a heat stabilized, flame retardant, self-extinguishing engineering thermoplastic, reinforced with glass-fiber 30% (by weight) based on a semi-crystalline Polyamide-66- Polyamide-6-alloy. Grilon TSG-30/4 V0 is halogen-free and free of red phosphorus. The unpigmented material is of light inherent color. Besides its advantageous flame behavior, Grilon TSG-30/4 V0 exhibits high toughness and generally good mechanical properties.

RoHS: Grilon TSG-30/4 V0 complies with the regulations acc. RoHS (2002/95/EC, Restriction of Hazardous Substances).

WEEE: Parts made of Grilon TSG-30/4 V0 are not affected by the demands for "selective recycling" acc. guideline 2002/96/EC for Electro and Electronic Appliances Grilon TSG-30/4 V0 is particularly suited for technical injection molded parts in the field of Electro and Electronics which require a flammability rating of V-0 acc. UL 94.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccDry; ISO 1183
Water Absorption 4.0 %Sim. to ISO 62
Moisture Absorption 1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 130 MPaConditioned; ISO 2039-1
 255 MPaDry; ISO 2039-1
Tensile Strength at Break 90.0 MPaConditioned; ISO 527-1/-2
 150 MPaDry; ISO 527-1/-2
Elongation at Break 2.5 %Dry; ISO 527-1/-2
 4.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 6500 MPaConditioned; ISO 527-1/-2
 10500 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 60.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 65.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 70.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 8.50 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 9.50 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °CLong Term; ISO 2578
 220 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 235 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 165 °CISO 75-1/-2
Flammability, UL94 V-0IEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
Burning BehaviorVDE
Electricals & ElectronicsCables & Tubes
 Connectors
 Electrical appliances
 Electrical equipment
 Energy distribution
 Lighting
FormGranules
ProcessingInjection Molding
Special CharacteristicsFlame retardant
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Conditioned)
Celanese Celcon® M90™ POM, Unfilled
EMS-Grivory Grilamid® L 16 GM nat PA12
EMS-Grivory Grilamid® L 16 LM PA12
EMS-Grivory Grilamid® L 20 G PA12

PGRH266 / 156975

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.