Hostacom CA199AC BLK low melt flow, 400 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin exhibits balanced strength, toughness, flexibility and ductility. Applications: Automotive Parts, Interior Automotive Applications.Information provided by LyondellBasell. |