MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound QCL349 Polyamide 610 (Nylon 610)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: LNP LUBRICOMP QCL349 compound is based on Nylon 6/10 resin containing 15% PTFE, 20% carbon fiber. Added features of this grade include: Wear Resistant, Flame Retardant, Electrically Conductive.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Wear resistant,Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccASTM D792
 1.52 g/ccISO 1183
Moisture Absorption 0.100 %23°C/50% RH/24 hrs; ASTM D570
 0.120 - 0.200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0010 cm/cm24hrs; ASTM D955
 0.0011 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0078 cm/cm24hrs; ISO 294
 0.0080 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 158 MPaASTM D638
 162 MPaISO 527
Tensile Strength, Yield 162 MPaISO 527
 168 MPaASTM D638
Elongation at Break 1.6 %ISO 527
 1.9 %ASTM D638
Elongation at Yield 1.6 %ISO 527
 1.8 %ASTM D638
Tensile Modulus 15750 MPa1 mm/min; ISO 527
 16540 MPa50 mm/min; ASTM D638
Flexural Strength 239 MPaISO 178
 241 MPaASTM D790
Flexural Modulus 13000 MPaISO 178
 13100 MPaASTM D790
Izod Impact Notched 53.0 JASTM D256
Izod Impact, Unnotched 534 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 32.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 4.00 Jpeak; ASTM D3763
Impact Test 2.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.34ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.28ASTM D3702 Modified: Manual
K (wear) Factor 444 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 19.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 55.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 57.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 218 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 217 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 198 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 200 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 260 - 270 °C
Zone 3 270 - 280 °C
Melt Temperature 270 - 275 °CInjection Molding
Mold Temperature 80.0 - 95.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80945 / 288892

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.