MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond FS227 Thixotropic Epoxy/Polyamide Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-BOND FS227 is a thixotropic (thick paste) polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting, toughness, and superior mechanical properties are required. This easy-to-use, amber colored epoxy adhesive system has a moderate pot life and a low exotherm. It cures at room temperature, and develops strong bonds to most material surfaces, including many metals, rigid plastics, glass, ceramics, leather, rubber, wood and concrete. Fully cured TRA-BOND FS227 is a tough, resilient adhesive with good low temperature electrical, mechanical and impact resistant properties, superior thermal shock resistance, low permeability to gases and vapors, good dimensional stability and outstanding resistance to water, weather, oxygen and ozone, most petroleum products, mild acids and alkalis, and many other chemicals.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccMixed
Viscosity 600 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75
Tensile Strength, Yield 5400 psi
Elongation at Yield 10 %
Adhesive Bond Strength 2500 psiLap shear, alum to alum, 1 hr @ 100°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.20e+14 ohm-cm
Dielectric Constant 3.35
@Frequency 1000 Hz
Dielectric Strength 460 V/mil
Dissipation Factor 0.010
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 64.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 110 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 70.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 75 min
 
Descriptive Properties
Color Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 2248 High Temperature Epoxy Staking Adhesive
Tra-Con Tra-Bond 2212 High Temperature Epoxy Adhesive
Tra-Con Tra-Bond 2211 High Temperature Epoxy Adhesive

PTRAC272 / 71200

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.