MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-KON™ Compound DE0049P Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DE0049P compound is based on Polycarbonate (PC) resin containing 20% carbon fiber. Added features of this grade include: Electrically Conductive, Flame Retardant, Exceptional Processing.

Features: High Stiffness,Light-weight Structural,Superior Molding,Super Strong (Carbon Fiber Filled),Flame Retardant,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccASTM D792
 1.33 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0014 cm/cm24hrs; ISO 294
 0.0010 - 0.0030 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0056 cm/cm24hrs; ISO 294
 0.0050 - 0.0070 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 132 MPaISO 527
 137 MPaASTM D638
Elongation at Break 0.90 %ASTM D638
 1.3 %ISO 527
Tensile Modulus 15960 MPa1 mm/min; ISO 527
 16540 MPa50 mm/min; ASTM D638
Flexural Strength 193 MPaASTM D790
 219 MPaISO 178
Flexural Modulus 12410 MPaASTM D790
 13200 MPaISO 178
Izod Impact Notched 58.0 JASTM D256
Izod Impact, Unnotched 432 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 28.0 kJ/m²80*10*4; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 32.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 33.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 34.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 35.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 143 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 143 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 139 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 138 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-0
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 310 - 320 °C
Zone 3 320 - 330 °C
Melt Temperature 305 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81216 / 289163

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.