MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Solvay RHODOLINE® 670 Surfactant
Categories: Fluid

Material Notes: Description: Highly effective mineral oil defoamer for latex processing..

Identification: OIL BASE DEFOAMER

Available in: North America

Applications: RHODOLINE 670 is an APE-free and silicone–free defoamer with outstanding performance in a wide range of adhesives and latex applications, including Pressure Sensitive Adhesives, Vinyl Acetate, Poly Vinyl Alcohol and acrylic latex. RHODOLINE 670 is recommended for use at concentration of 0.1 to 0.5%. It can be used as received or pre-dispersed in water.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 - 0.920 g/ccRP-17617
pH 5.0 - 7.05% Solution; RP-0420
Viscosity 300 - 800 cPLV# @ 60 rpm; RP-0596
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceLight Tan Opaque LiquidRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parson Adhesives PARTITE® 7390 Methacrylate Structural Adhesive
Lucite International Colacryl® TS1778 Acrylic Solution Resin
Lord Adhesives 8400 Fast Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive
ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate
ExxonMobil 624 Mobil SHC 600 Series

WRHOD482 / 137713

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.