MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Shin-Etsu Silicones KE-541U Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: KE541U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending filler.

Product Features:

  • This product can be blended with KE551U, KE561U, KE571U, and KE581U for intermediate hardnesses. The choice between these bases will depend on specific requirements.
Typical Applications:
  • Roll covers.
  • Diaphragms.
  • O-rings and gaskets./ul>

    Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccDCBP Cure
 1.10 g/ccDBPH Cure
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40DBPH Cure
 42DCBP Cure
Tensile Strength at Break 1115 psiDCBP Cure
 1430 psiDBPH Cure
Elongation at Break 460 %DCBP Cure
 730 %DBPH Cure
100% Modulus 0.100 ksi
@Strain 100 %
DBPH Cure
 0.130 ksi
@Strain 100 %
DCBP Cure
Tear Strength 7.00 pliDie B; DBPH Cure
 74.0 pliDie B; DCBP Cure
Compression Set 13 %
@Temperature 150 °C,
Time 79200 sec
DCBP Cure
 
Descriptive Properties
Cure AgentDBPH
 DCBP
Cure TypePost Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shin-Etsu Silicones 541 Fluid
Shin-Etsu Silicones KE-1843 Silicone, RTV Adhesive/Sealant
Shin-Etsu Silicones KE-3421 Silicone, RTV Conformal Coating
Shin-Etsu Silicones KE-3475TUV Silicone, RTV Conformal Coating
Shin-Etsu Silicones KE-3479 Silicone, RTV

PSHIN222 / 177733

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.