MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCast 7703-21/AboCure 7703-21 (A) Epoxy Adhesive and Casting Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permanently to metal, wood, glass, fiberglass, ceramics, rigid plastics, concrete, marble, stones, and jewelry. It is excellent to laminate fiberglass, metal sheets, paper or canvas, or any other material for composite structures. As a Dielectric: widely used for potting, encapsulating, dipping, insulating circuits, chips, and other components. As a Casting Resin: for filling, embedments, reproductions, tooling (as is, or blended with fillers such as metal powders, sawdust, etc.). This compound is virtually unaffected by average ambient conditions, soft and salt water, alkalis and diluted acids, several solvents, detergents, oils and greases. Final properties can be modified by changing the AboCast/AboCure ratios: the highest rigidity, hardness, chemical and heat resistance are offered by the 1400/40 ratio. Higher AboCure ratios (up to 100/100 parts AboCast/AboCure) yield increasing flexibility, shock and thermocycling resistance, and adhesion to problem surfaces. The 7703-21 System develops tenacious adhesion to metals, ceramics, wood, fiberglass, masonry, and most materials to form permanent structural and dielectric bonds. Radiation resistance recommends the 7703-21 System in X-ray and other radioactive environments.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 4000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87
Tensile Strength, Ultimate 8800 psi
Elongation at Break 5.8 %
Izod Impact, Notched 0.500 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.50e+11 ohm-cm
@Temperature 93.0 °C
 4.40e+13 ohm-cm
@Temperature 66.0 °C
 1.00e+16 ohm-cm
@Temperature 25.0 °C
Dielectric Constant 3.57
@Frequency 1e+6 Hz
Dissipation Factor 0.021
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 75.0 °CDeflection Temp at unknown load
 
Processing PropertiesOriginal ValueComments
Pot Life 80 - 120 min
 
Descriptive Properties
Hardening Time (min)60-240castings
 720-2880adhesive
Parts by Weight (pbw)100AboCast
 40AboCure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Chemfab® 1580 PTFE Coated Fiberglass Conveyor Belting
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting
Mitsubishi Chemical Advanced Materials Ketron™ CM GF30 Compression Molded, 30% Glass Reinforced Polyetherether Ketone
Saint-Gobain Chemfab® 3 Industrial PTFE-Coated Glass
Fiberglass Grade B

PABC878 / 107862

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.