MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mateck Glass (BK7 analogous)
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.51 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 81.0 GPa
Poissons Ratio 0.206
Shear Modulus 33.6 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.10 µm/m-°C
@Temperature -30.0 - 70.0 °C
Specific Heat Capacity 0.858 J/g-°C
Thermal Conductivity 1.114 W/m-K
Melting Point 559 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.50731
@Wavelength 1014 nm
 1.51872
@Wavelength 546.1 nm
at ne
 1.52283
@Wavelength 480 nm
at nf'
 1.53626
@Wavelength 365 nm
IR Transmittance 75 %
@Wavelength 2300 nm
Internal Transmittance
 90 %
@Wavelength 2000 nm
Internal Transmittance
UV Transmittance 8.0 %
@Wavelength 300 nm
Internal Transmittance
 92 %
@Wavelength 350 nm
Internal Transmittance
 
Descriptive Properties
Thermal Coefficient of Refractive Index2.8E-060.546 microns for ± 20°C
Transmission Range (microns)0.35 - 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott N-BK7 Glass
Schott P-BK7 516641.243, Optical Glass
724-8 Nextrema® Opaque White Glass Ceramic/SCHOTT
Borosilicate Glass
Mateck Zero Expansion Glass - ZERODUR

CMAT044 / 87728

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.