SABIC® Vestolen A 5061R 10000 (black) is a grade, which has a high densityand a bimodal distribution of the molecular mass. An universal grade for pipe extrusion which, due to a keen combination of properties, is typically used for drinking water and waste water piping.
This material meets (inter)national standards for use in drinking water and wastewater piping.
MRS class ISO 12162 MPa = 8.0 (PE 80).
This product is not intended for and must not be used in any pharmaceutical/medical applications.Information provided by SABIC |