MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Crucible Steel CSM® 6 Tool Steel, AISI A6
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel

Material Notes: CSM 6 is an air hardening tool steel offering moderate wear resistance and toughness. It may be hardened from a low hardening temperature for easy heat treatment.

Information provided by Crucible Industries

Key Words: AISI A6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.283 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 217 - 248
Hardness, Rockwell C 48
@Tempering Temp. 538 °C
hardened at 1855°F then tempered
 50
@Tempering Temp. 482 °C
hardened at 1855°F then tempered
 52
@Tempering Temp. 427 °C
hardened at 1855°F then tempered
 54
@Tempering Temp. 371 °C
hardened at 1855°F then tempered
 55
@Tempering Temp. 316 °C
hardened at 1855°F then tempered
 56
@Tempering Temp. 260 °C
hardened at 1855°F then tempered
 58
@Tempering Temp. 204 °C
hardened at 1855°F then tempered
 60
@Tempering Temp. 149 °C
hardened at 1855°F then tempered
 61
@Tempering Temp. 93.3 °C
hardened at 1855°F then tempered
Modulus of Elasticity 30000 ksi
Charpy Impact 27.0 ft-lb
@Tempering Temp. 149 °C
austenitized at 1550°F then tempered; C-notch
 44.0 ft-lb
@Tempering Temp. 204 °C
austenitized at 1550°F then tempered; C-notch
 60.0 ft-lb
@Tempering Temp. 260 °C
austenitized at 1550°F then tempered; C-notch
 67.0 ft-lb
@Tempering Temp. 316 °C
austenitized at 1550°F then tempered; C-notch
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.60 µin/in-°F
@Temperature 20.0 - 93.3 °C
 6.90 µin/in-°F
@Temperature 20.0 - 204 °C
 7.20 µin/in-°F
@Temperature 20.0 - 316 °C
 7.50 µin/in-°F
@Temperature 20.0 - 427 °C
 7.70 µin/in-°F
@Temperature 20.0 - 538 °C
Thermal Conductivity 216 - 228 BTU-in/hr-ft²-°F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.70 %
Chromium, Cr 1.0 %
Iron, Fe 94.65 %as balance
Manganese, Mn 2.0 %
Molybdenum, Mo 1.35 %
Silicon, Si 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type H22 Tungsten Hot Work Tool Steel (UNS T20822)
Ampco Metal AMPCO® 26 Aluminum Bronze, Forging
Kinetics MIM 4605 Low Alloy Steel (As Sintered)
AISI Type A6 Tool Steel
AISI Type A2 Tool Steel

NCRUC910 / 160361

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.