MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Anderol ANDEROL® FGC 5 Fluid, Synthetic Mechanical Seal Fluid ISO 22  (discontinued **)
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Description: ANDEROL FGC 5 Mechanical Seal Fluid is a synthetic hydrocarbon (PAO) based lubricant. FGC 5 Fluid meets the former H-1 approval requirements of the USDA where incidental food contact can occur. ANDEROL food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. ANDEROL food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.” The Islamic Food and Nutrition Council of America (IFANCA) endorses FGC 5 Fluid as being produced in conformity with all requirements of Halal.

Information provided by ConocoPhillips.

Anderol® is a registered trademark of The Anderol Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.830 g/cc
@Temperature 15.6 °C
0.830 g/cc
@Temperature 60.0 °F
60°F; ASTM D-1298
Saybolt Viscosity at 100°F 100 SUS100 SUSASTM D-2161
Saybolt Viscosity at 210°F 40 SUS40 SUSASTM D-2161
Kinematic Viscosity at 40°C (104°F) 20.9 cSt20.9 cStASTM D-445
Kinematic Viscosity at 100°C (212°F) 4.0 cSt4.0 cStASTM D-445
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.600 mm0.0236 in1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172
 
Thermal PropertiesMetricEnglishComments
Pour Point -60.0 °C-76.0 °FASTM D-97
Flash Point 240 °C464 °FASTM D-92
 
Compliance PropertiesMetricEnglishComments
USDA YesYes
 
Descriptive Properties
Copper Corrosion1A3 hrs. at 100°C, ASTM D130
Demulsibility (40-40-0)Max 30 minutesat 54°C, ml oil/water/emulsion, ASTM D1401
EvaporationMax 1.0 %ASTM D-972, 22 hrs. @ 99°C (210°F)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Syncon® 32 Synthetic AW Hydraulic Fluid 32
Phillips 66 32 Super Hydraulic Oil
ExxonMobil SpectraSyn™ 2 Polyalphaolefin (PAO) Fluid
ExxonMobil Mobil Synturion 6
ChevronTexaco TEGRA® Synthetic Barrier Fluid

WCON290 / 75327

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.