For production of resin KFMT-15, KF-0, KF-Z etc., which contain up to 70% of dry residue. 40-44% general formaldehyde content. 24-26 general carbamide content. Full solubility in water at 20°C in ratio 1:20. 5.5-7.5 pH concentration of hydrogen ions. |