MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm ACRYLITE® Optical Acrylic Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: ACRYLITE® Optical hard coat is unlike any other hard coated flat acrylic sheet in the market. Using a proprietary application method, our one side hard coated sheet offers exceptional optical clarity and surface quality with an excellent abrasion and chemical resistant coating. Perfect for demanding environments, ACRYLITE® Optical hard coat is the right choice for any application that requires heavy wear and tear and frequent cleaning.

Properties: General properties of ACRYLITE® include:

  • excellent light transmission and brilliance
  • outstanding weather resistance
  • easy to fabricate
  • high surface hardness
  • light weight – half the weight of glass
  • 11 times more break resistant than glass
ACRYLITE® Optical hard coat offers the following additional product benefits:
  • excellent surface appearance
  • excellent resistance to abrasion and Chemicals
Applications: digital printing & signage
  • furniture & retail/POP displays
  • gaming & vending machines
  • picture framing
  • aviation (dust covers for windows)
  • electronic displays
  • industrial glazing

    Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength at Break 68.1 MPa9880 psiASTM D638
    Modulus of Elasticity 2.76 GPa400 ksiASTM D638
    Izod Impact, Notched (ISO) 0.400 kJ/m²0.190 ft-lb/in²ASTM D256
     
    Thermal PropertiesMetricEnglishComments
    Vicat Softening Point 104 °C219 °FASTM D1525
     
    Optical PropertiesMetricEnglishComments
    Yellow Index <= 0.50 %<= 0.50 %DIN 5036
    Transmission, Visible 92 %92 %ISO 13458-2

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Röhm Acrylite® 8N Acrylic Polymer
    Röhm Acrylite Plus® zdf Impact Acrylic Polymer
    Röhm Acrylite Plus® zk3HR Impact Acrylic Polymer
    Röhm Acrylite Plus® zk4BR Impact Acrylic Polymer
    Röhm Acrylite Plus® zk4HR Impact Acrylic Polymer

    PEVONIL058 / 196262

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.