MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
ALIMEX AMP 8000 Aluminum Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: AMP 8000 offers higher strength levels, good machinability and dimensional stability. Its tensile strength is up to 40% higher than AlZn5.5MgCu (7075).

Moulding, (Prototypes) injection moulds, Jig and fixture manufacturing, Tool manufacturing, Special machine construction, Standard parts. Information provided by ALIMEX GmbH

Key Words: Aluminium alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.1022 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 145 - 180
Tensile Strength, Ultimate 460 - 590 MPaRm
Tensile Strength, Yield 400 - 555 MPa
@Strain 0.2 %
Elongation at Break 4.0 - 11.5 %
Modulus of Elasticity 71.0 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 1145.1 BTU-in/hr-ft²-°F
 
Descriptive Properties
Machinability Good
Polishing PropertiesGood
Protective AnodizingNot decorative
Welding Properties (WIG, MIG)Suitable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for 4000 Series Aluminum Alloy
Overview of materials for 6000 Series Aluminum Alloy
Overview of materials for 7000 Series Aluminum Alloy
Aluminum 6061-O
Overview of materials for 5000 Series Aluminum Alloy

NALIMEX07 / 14762

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.