Introduction: Emulsion EM1065 is a water dilutable 60% silicone fluid emulsion, employed as a releasing agent for rubber and generally plastic materials. In art graphic industry it is mainly used as antistatic and slip agent, it confers resistance to scratching during paper folding processes and protection to mechanical components. Features and Benefits - General purpose release agent
- Minimum build-up on mould
- Moulded parts not discoloured
- Good dilution stability
- Good lubricant and antistatic properties
- Chemically inert
Applications : Emulsion EM 1065 has been formulated specially as a release agent and lubricant in a wide range of applications and processes such as: - mould release agent
- release agent for bandaging of rubber tubes in vulcanisation process
- textile lubricant for yarn and thread as well as hosiery manufacture
- lubricant and antistatic in rotogravure off-set printing
- release agent for plastic tubes used to form bags and sacks
- gloss, slip and wettability in detergent and cleaner formulations
Information provided by CHT Group |