MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID 66 GF 33 TS PA66, 33% glass fibre, thermal stability
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Features

PA 66 for injection moulding, chemically reinforced with 33% glass fibre, heat stabilized, suitable for high strength and high impacted mouldings. Used in automotive, engineering and electrical industry. Can be used in environment, in which longtime heat impact of up to 200°C occurs. Decrease in tensile s trength by 50 % after 5000 hours at 170°C. The heat stabilization predetermines the products to environment with longtime heat exposure, like eg. intake pipes, cylinder heads, induction coils, carrying parts in the motor fixing in the motor area. Application: hobby tools, gears, covers of electric tools, cooling water distribution in the automotive industry. Delivered in black.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/cc
Viscosity Measurement 0.71 - 1.05
Linear Mold Shrinkage 0.0071 cm/cm
Linear Mold Shrinkage, Transverse 0.0105 cm/cm
Melt Flow 3.0 g/10 min
@Load 0.325 kg,
Temperature 270 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPa
Elongation at Break 2.0 %
Tensile Modulus 11000 MPa
Flexural Strength 265 MPa
Flexural Modulus 10000 MPa
Charpy Impact Unnotched 75.0 kJ/m²
@Temperature -20.0 °C
 90.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 12.0 kJ/m²
@Temperature -20.0 °C
 13.0 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
Dielectric Strength 50.0 kV/mm
Comparative Tracking Index 400 V
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
Vicat Softening Point 250 °CB
Flammability, UL94 HB
Glow Wire Test 650 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.15 %
Injection Pressure 70.0 - 120 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celcon® GB25 POM, 25% Glass Reinforced
DuPont Mobility and Materials Zytel® 70G35HSRX BK099 PA66-GF35
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Conditioned)
Global Atron 6602 GF-33 Black Industrial Nylon 66, 33% Glass Filled
BASF Ultramid® N-333 NF3001 33% Glass Filled PA66 (Dry)

PPLACO416 / 121040

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.