MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Polyram PlusTek PB826G3 Nylon 6 for Injection Molding, 15% Glass-fiber Reinforced, Impact Modified and UV Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: 15% Glass fiber reinforced, impact modified and UV stabilized Nylon 6 for injection molding applications.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183
Moisture Absorption at Equilibrium 2.5 %50% RH; ISO 62
Water Absorption at Saturation 7.3 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 85
Tensile Strength, Yield 100 MPaISO 527
Elongation at Break 3.5 %ISO 527
Tensile Modulus 4900 MPaISO 527
Flexural Strength 150 MPaISO 178
Flexural Modulus 4200 MPaISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature -70.0 °C
ISO 179
 72.0 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179
 20.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
Dielectric Strength 80.0 kV/mmIEC 60250
 
Thermal PropertiesOriginal ValueComments
Melting Point 218 °CISO 11357
Maximum Service Temperature, Air 110 °CContinuous use
 200 °CShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 170 °CISO 75
Vicat Softening Point 215 °CISO 306
Flammability, UL94 HB
@Thickness 3.00 mm
Flame Spread 20 mm/minFMVSS302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nurel Engineering Polymers Promyde® B30 P2 G15 MI PA 6, Dry, 15% Glass Reinforced, Injection Molded, Impact modified and Heat Stabilized
Nurel Engineering Polymers Promyde® B30 P2 G15 MI PA 6, Conditioned, 15% Glass Reinforced, Injection Molded, Impact modified and Heat Stabilized
Celanese Zytel® 80G14AHS NC010 PA66-IGF14
Toyobo PELPRENE™ S3001 Polyester TPE
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified

PPOLYR820 / 126619

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.