MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt HUP 27/25 RN-9010 Aircraft Homologate
Categories: Polymer; Thermoset; Polyester, TS

Material Notes:

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.93 g/ccISO 1183 A
Filler Content 25 %Fiber; ISO 1172
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 60.0 MPaISO 527-4
Flexural Strength 150 MPaISO 14125
Flexural Modulus 9000 MPaISO 14125
Tensile Impact Strength 60.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CIEC 60216
Flammability, UL94 V-0
@Thickness 2.50 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature >= 145 °C
Hold Pressure >= 1450 psiMolding pressure
Cure Time 90.0 secISO 12114/1
 
Descriptive Properties
Fiber length25 mmDF PA3.01
Molding time> 25 sec./mm
Surface Weight3000 g/m2ISO 10352

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Rohacell® 51 A Aircraft Grade Polymethacrylimide (PMI) Foam
Evonik Rohacell® 110 A Aircraft Grade Polymethacrylimide (PMI) Foam
ChevronTexaco ISO 22 Form Oil
ChevronTexaco 120 Aircraft Engine Oils

PPOLYN9034 / 231629

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.