MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated
Categories: Polymer; Thermoset; Epoxy

Material Notes: HYTAC-WFT combines the higher temperature, smooth surface properties of HYTAC-WF with PTFE impregnation for low stick surface capability and excellent material distribution. The result is a syntactic plug assist material with a service temperature of 4250F that may be polished to an ultra-smooth surface.

The intended uses of HYTAC-WFT are for difficult sheet sticking problems or in situations where an extremely smooth surface is critical to part quality.

As with other syntactic materials, HYTAC-WFT offers the following advantages:

  • Low thermal conductivity and specific heat
  • Dimensionally stable
  • Excellent temperature resistance
  • Lightweight
  • Easily machined
Variety of Shapes and Sizes: The material is provided in standard sized rods or sheets, but may be custom molded to meet the specific needs.

Applications: HYTAC-WFT machines and polishes to an ultra-smooth finish.

Recommended for use with CPET, EVOH, LDPE, PC, PMMA, PS and RPET

Information Provided by CMT Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 50.0 - 60.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Flexural Toughness 4.50 psiASTM D790
Compressive Strength 17500 psi
Compressive Modulus 325 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.4 µin/in-°F
Thermal Conductivity 0.190 W/m-K
Maximum Service Temperature, Air 425 °F
 
Descriptive Properties
ColorLight Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMT Materials HYTAC® FLXT High Temperature, PTFE Impregnated Copolymer Syntactic
Aptek DIS-A-PASTE 2310-PMF Thermally conductive adhesive/encapsulant
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
CMT Materials HYTAC® B Solid Polymer Tooling Material
Chi Mei Wonderlite® PC-110 Polycarbonate

PCMT003 / 93140

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.