MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Trigonox 101-SC8B 2,5-Dimethyl-2,5-di(tert-butylperoxy)hexane, gum in silicone rubber
Categories: Other Engineering Material

Material Notes: Trigonox 101-SC8B is a bifunctional peroxide formulation which is mainly used for the crosslinking of silicone rubbers.

CAS number: 78-63-7; 68083-18-1

EINECS/ELINCS No: 201-128-1; not listed

Applications: Trigonox 101- SC8B is mainly used for the crosslinking of silicone rubbers. Rubber compounds containing Trigonox 101- SC8B have excellent scorch safety. Safe processing temperature: 135°C (rheometer ts2 > 20 minutes). Typical crosslinking temperature: 175°C (rheometer t90 about 12 minutes).

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 290.4 g/mol290.4 g/mol
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 80.0 °C176 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Content (%)11.02Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY982 / 286505

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.