MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Global EPP PA 6C HS BLUE Cast Polyamide 6 + UV and Heat Stabilizers
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of cast nylons may be altered to suit specific applications, and the performance of the basic polymer can be enhanced with the addition of various additives, fillers, lubricants and colorants.

Key characteristics:

  • Unequalled formulation options and profile range
  • Excellent mechanical, thermal and chemical resistance
  • Excellent PV and load bearing capabilities
  • Excellent wear and abrasion resistance
  • Good dimensional stability, largely free from internal stresses
  • FDA compliant grades available

Additives in the form of high temperature resistant colorants, heat and UV stabilisers allow this material to better retain mechanical properties in applications operating at higher temperatures. The inorganic dye used to produce HS BLUE’S distinctive colour conforms to the specifications required by the Japanese market for cast nylon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccTest Method A; ISO 1183:1987
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
Immersion; ISO 62:1999 (modified)
Water Absorption at Saturation 5.3 %ISO 62:1999
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84ISO 868:2003
Tensile Strength at Break 80.0 MPaSample Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 20 %Sample Type 1B, 50 mm/min; ISO 527-1/2:1993
Modulus of Elasticity 4.00 GPaSample Type 1B, 50 mm/min; ISO 527-1/2:1993
Flexural Strength 105 MPa1.5 mm/min; ISO 178:2001
Flexural Modulus 3300 MPa1.5 mm/min; ISO 178:2001
Compressive Strength 95.0 MPaSample Type B, 5 mm/min; ISO 604:2002
Compressive Modulus 2700 MPaSample Type A, 1 mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 5.40 kJ/m²Sample Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.15
@Pressure 1.75 MPa
31.4 m/min
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance 1.00e+12 ohmIEC 60093:1980-01
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 60250:1969-01
 4.0
@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mmIEC 60243-1:1998-01
Comparative Tracking Index 600 VIEC 60112:2003-01
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-2:1999
Melting Point 220 °C
Maximum Service Temperature, Air 115 °CContinuous
 180 °CIntermittent
Minimum Service Temperature, Air -100 °CIntermittent
 -40.0 °CContinuous
Flammability, UL94 HBIEC 60695-11-10:2003-08
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Tecamid® HS Nylon (PA)
Edinburg Plastics HTT605 PA 6 Impact Modified
Edinburg Plastics HGT605 PA 6 Impact Modified
CP-Polymer-Technik Wellamid® 6000/58 CP Nylon 6, Impact Modified Until -40°C, Dry
CP-Polymer-Technik Wellamid® 6000/58 CP Nylon 6, Impact Modified Until -40°C, Conditioned

PGLOEPP04 / 79515

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.