MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID 66 CF 30 PA66, 30% carbon fibre  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Carbon Fiber Filled

Material Notes: Features

Chemically reinforced with 30% carbon fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. Delivered in black color.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/cc
Viscosity Measurement 0.11 - 0.48
Linear Mold Shrinkage 0.0011 cm/cm
Linear Mold Shrinkage, Transverse 0.0048 cm/cm
Melt Flow 1.0 g/10 min
@Load 0.325 kg,
Temperature 270 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPa
Elongation at Break 4.0 %
Tensile Modulus 16000 MPa
Flexural Strength 290 MPa
Flexural Modulus 15300 MPa
Charpy Impact Unnotched 65.0 kJ/m²
@Temperature -20.0 °C
 75.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -20.0 °C
 11.0 kJ/m²
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
Vicat Softening Point 240 °CB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °C
Mold Temperature 80.0 - 90.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.15 %
Injection Pressure 70.0 - 120 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 CF 30 TS PA 66 reinforced with 30% carbon fibre, thermal stabilization
VICTREX™ PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Plastcom SLOVAMID 6 CF 20 PA6, 20% carbon fibre
Plastcom SLOVAMID 6/66 CF 30 PA6/66, 30% carbon fibre
Plastcom SLOVAMID 66 CF 40 PA66, 40% carbon fibre

PPLACO432 / 121056

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.