MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution PS 456EB HIPS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Styrolution PS 456EB is a high flow, high impact polystyrene with a good heat resistance and a high stiffness, developed for injection blow molding applications, especially for bottle of yogurt.
  • High flow
  • Injection blow molding applications

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Moisture Absorption at Equilibrium <= 0.10 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation <= 0.10 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 in/inISO 294-4
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 90.0 MPaISO 2039-1
Tensile Strength, Yield 23.0 MPaISO 527
Elongation at Break 40 %ISO 527
Elongation at Yield 1.5 %ISO 527
Tensile Modulus 2000 MPaISO 527
Flexural Strength 42.0 MPaISO 178
Flexural Modulus 2100 MPaISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 120 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 11.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+18 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 155 kV/mm
@Thickness 1.50 mm
Short Time; IEC 60243-1
Dissipation Factor 0.00040
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°CISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °CISO 75
Vicat Softening Point 86.0 °C
@Load 5.10 kg
50°C/h; ISO 306
 94.0 °C
@Load 1.02 kg
50°C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 260 °CISO 294
Mold Temperature 10.0 - 60.0 °CISO 294
Injection Velocity 200 mm/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution PS 5600/5601 HIPS
Chevron Phillips MA5350 HIPS - High Impact Polystyrene
INEOS Styrolution PS 576H HIPS
INEOS Styrolution PS 2710 HIPS
Dow AIM® 4800 High Impact Styrenic Resin

PBASG1090 / 159636

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.