MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vikas Ecotech ADDFLEX ESO 603 Epoxidized Soyabean Oil
Categories: Other Engineering Material

Material Notes: Product Description: ADDFLEX, and Epoxidized Soyabean Oil, is a High Oxirane Content, Efficient & Compatible Vinyl Additive which essentially functions similar to a polymeric type plasticizer by imparting flexibility and controlling migration due to its high molecular weight. It is also a synergetic, heat & light stabilizing additive that compliments the conventional Metallic Stabilizer systems, facilitating superior processing ability and cost reduction.

Characteristics & Usages: ADDFLEX is recommended particularly for formulations such as:

  • Efficient Plasticization of all flexible & semiflexible PVC Compounds & Emulsions
  • Supplementing Heat & Light stabilization of Rigid, Semi Rigid & Flexible PVC Compounds
  • Heat Stabilization of CPW plasticizers during the manufacturing process
  • Plasticization of Neoprene, Nitrocellulose and Chlorinated Rubber
  • Facilitating homogenous pigment dispersions
  • Better Processabilty & Output in rigid PVC Compounds
  • Improving Oil & Gas Resistivity
CAS No: 8013-07-8

Information provided by Vikas Ecotech LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.985 - 0.995 g/cc0.985 - 0.995 g/ccHydrometer
Viscosity Measure 450 - 500 cSt450 - 500 cStOstwald Viscometer (U Tube)
Maximum Moisture Content 0.150.15
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 1.0<= 1.0[mg KOH/g]; IS 548
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 305 °C>= 581 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.471 - 1.4751.471 - 1.475
Gardner Color Number <= 2.0<= 2.0
 
Descriptive Properties
AppearanceClear Pale Yellow Liquid
Iodine Value1.5-3.5 gl2/100gWij's method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVICAS003 / 285416

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.