Formulated TPE compound is based on Shell's Kraton G resin and is widely used in automotive applications exhibiting a wide temperature range, replacing in many applications conventional thermoset rubber. Multibase is a licensed compounder for Shell's Kraton G polymers. Multi-Flex TPE contains Kraton™ G. Data provided by Multibase. |