MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Paliogen® Red L 3885 Color Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Transparent perylene red with a very clean shad

Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Airdrying systems.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³
Specific Surface Area 53 m²/g53 m²/g
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 5.0 - 8.05.0 - 8.0
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 5000 ohm-cm>= 5000 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 300 °C572 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Descriptive Properties
Chemical Fastness (months)Butylacetate5
 Ethanol5
 HCL 2%5
 Methyl ethyl ketone4-5
 Mineral spirits5
 NaOH 2%5
 Solvenon™PM4-5
 Xylene5
ColorRed
Fastness to Overcoating5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borosilicate Glass
Corning Gorilla® Glass 5 Display Glass
MarkeTech AO 98 Aluminum Oxide Ceramic Substrate, 98% Purity
MarkeTech AO 95 Aluminum Oxide Ceramic Substrate, 95% Purity
MarkeTech AN 120 Aluminum Nitride Ceramic Substrate, 98% Purity

PBASG0754 / 132387

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.