MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Silres® BS 30 Silicone Resin
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® BS 30 A is a stable, VOC compliant, 100% actives siloxanes/ silicone resin blend that imparts water and stain repellency to substrates while providing an enhanced look. SILRES® BS 30 A, currently produced in the USA, was developed to treat a wide variety of mineral substrates commonly used in the tile industry including tumbled marble , limestone, slate, and saltillo clay tile.

Special features:

  • Provides excellent water repellency to reduce cracking, spalling, freeze/thaw damage, chemical degradation, biological growth, efflorescence, and dirt pickup, thereby lengthening substrate life and reducing maintenance costs.
  • Provides excellent stain repellency to reduce chemical degradation and biological growth for improved aesthetics, thereby lengthening substrate life and reducing maintenance time and expenses.
  • Superior storage stability including freeze/thaw stability for ease of use.
  • Low VOC emissions upon curing.
  • Formulated to impart an enhanced appearance on stone and natural tile substrates.
  • Formulated to provide either a matte finish or a gloss finish, depending upon application.
  • Physically and chemically bonds to substrates increasing coating life and making cleaning easier, thereby reducing maintenance costs.
  • Coatings are UV stable and resistant to biological degradation for longer service life leading to less cost for repetitive applications.
  • Coatings are vapor permeable to resist cracking, peeling and blistering.
Application: SILRES® BS 30 A should be applied as supplied to achieve the desired application effect. One to two coats of the solution should be applied to achieve an enhanced appearance. Two to three coats of the solution should be applied to achieve an enhanced appearance with gloss. SILRES® BS 30 A can be applied with a soft, lint-free cloth, sponge, or paint brush. Excess material should be removed to prevent inconsistencies in the enhancement. The product should be fully curedwithin 24 hours. A test patch should be performed prior to general application with the customer's approval to ensure the desired appearance is achieved.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 - 1.06 g/ccWSTM 3019
Viscosity <= 100 cPWSTM-3342
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 93.3 °CWSTM-3322
 
Descriptive Properties
Content (%)100Silicone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silver-Magnesium-Nickel Alloy Strip (Ag-0.25Ni-0.25Mg), Soft Temper
Tantalum, Ta; Annealed
Silver-Magnesium-Nickel Alloy Strip (Ag-0.25Ni-0.25Mg), 3/4 Hard Temper
Silver, Ag; Commercially Pure (UNS P07020)
Silver, Ag

PWACK9533 / 205062

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.