MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Maxxam™ FR PP CONC 36 NAT S Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.

MAXXAM FR PP CONC 36 NAT S is designed to impart good flame retardancy to polypropylene. Because there are so many varieties of polypropylene, it is difficult to predict the required let-down ratio required to meet the specific flammability standards. When the concentrate is let down at the proper ratio the resulting material can achieve flame retardancy equivalent to the requirements for UL94 V-2 or UL94 V-0. For starting point formulations we would suggest 7 to 8 parts by weight of polypropylene to 1 part of Conc 36 for UL94 V-2 performance and 2 to 3 parts by weight polypropylene to 1 part of Conc 36 for UL94 V-0 performance at thicknesses between 0.75 and 3.0 mm.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Melt Flow 70 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Procedure A; ASTM D1238
 
Descriptive Properties
FeaturesFlame Retardant
FormsPellets
Generic MaterialPP, Unspecified
Generic NamePolypropylene, Unspecified (PP, Unspecified)
Regional AvailabilityNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding
Avient Maxxam™ FR PE CONC 1 Polyethylene, Low Density (LDPE)
Avient Maxxam™ FR PE 161-1A Polyethylene, High Density (HDPE)
Avient Maxxam™ FR PP FR 7A11 Polypropylene
Avient Maxxam™ FR PP FR 7C11 Polypropylene

PH0POL1106 / 145675

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.