Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Filler/Reinforcement: Glass Fiber, 40% Filler by Weight Features: Alcohol Resistant; Aromatic; Copolymer; Good Flow; Good Heat Resistance; Good Mold Release; Hydrolysis Resistant; Renewable Resource Content Uses: Appliance Components; Connectors; Electrical/Electronic Applications; Household Goods; Power/Other Tools Appearance: Black Forms: Granules Processing Method: Injection Molding Information provided by EMS-Grivory |