MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polymer Industries Polyslick UHMW Profile
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Polyslick UHMW Profiles exhibit all of the durable qualities of our Polyslick UHMW Sheet making them perfect for use where sheet stock is not suitable. Polymer Industries offers a large variety of profiles such as angles, channels, U shapes, tubing, and strips sold in coils. Some of our offerings fit conveyors for use as wear strips for specific applications. Polymer Industries will even develop custom profiles for customers with large requirements.

Information provided by Polymer Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccISO 1183
Water Absorption <= 0.010 %ISO 62
Viscosity Test 3850 cm³/gISO 307, 1157, 1628
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 17.0 MPaISO 527-2/1A
Elongation at Break >= 50 %ISO 527-2/1A
Elongation at Yield <= 20 %ISO 527-2/1A
Tensile Modulus 0.680 GPaISO 527-2/1A
Tensile Creep Modulus, 1 hour 430 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 220 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cmIEC 60093
Surface Resistance >= 1.00e+12 ohmIEC 60093
Dielectric Constant 2.1
@Frequency 100 Hz
IEC 60250
 3.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 45.0 kV/mmIEC 60243-1
Dissipation Factor 0.00029
@Frequency 100 Hz
IEC 60250
 0.0010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 20.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °CISO 75-1/-2
Vicat Softening Point 80.0 °CISO 306
Flammability, UL94 HB
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymer Industries Polyslick UHMW Sheet
Röchling Polystone® M MPG Glass filled UHMW-PE
Mitsubishi Chemical Advanced Materials TIVAR™ 88 UHMW-PE, Premium Glass Filled, Crosslinked Linings
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film
Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE)

PPOLIND16 / 56992

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.