MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Label-Lyte™ 25LL-101 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as overlaminates in pressure-sensitive labeling applications. This film is formulated with a proprietary non-migratory slip system. The treated clear layer provides excellent anchorage to most adhesives and is the intended print and laminating surfaces.

Availability: Latin America, North America and South America

Key Features:

  • Outstanding clarity and gloss
  • Excellent ink adhesion with most solvent-based and water-water-based ink systems
  • Excellent bond strength with most laminating adhesives
Applications:
  • Beverage, Carbonated
  • Beverage, Mineral Waters
  • Dairy Products
  • Dry Foods and Beverage Powders
Uses:
  • Pressure Sensitive Labels
Processing Method: Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 microns1.00 milExxonMobil Method
Coating Weight 22.7 g/m²14.2 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 147 %147 %20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 45 %45 %20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Coefficient of Friction 0.190.19Machinable; ExxonMobil Method
Film Tensile Strength at Break, MD 124 MPa18000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 241 MPa35000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 4.0 %
@Temperature 135 °C
4.0 %
@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 4.0 %
@Temperature 135 °C
4.0 %
@Temperature 275 °F
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ExxonMobil Method
Gloss 87 %87 %45°, Machinable Surface; ExxonMobil Method
 
Descriptive Properties
Wetting Tension0.83 receding cos thetaPrint Surface
Yield30500 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX99547 / 175783

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.