MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC XENOY™ X4850 PC+PBT (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: XENOY X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional stability. The X4850 could be positioned for body panels, safety equipment,housings, doorhandles, spring-loaded applications, medical device enclosures, outdoor sports equipment.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Density 1.31 g/ccISO 1183
Water Absorption 0.42 %23°C/sat; ISO 62
Moisture Absorption 0.140 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 4.5 g/10 min
@Load 5.00 kg,
Temperature 266 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 105 MPaISO 2039-1
Tensile Strength at Break 45.0 MPa50 mm/min; ISO 527
 50.0 MPa5 mm/min; ISO 527
 55.0 MPa50 mm/min; ASTM D638
 60.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 58.0 MPa5 mm/min; ASTM D638
 58.0 MPa5 mm/min; ISO 527
 63.0 MPa50 mm/min; ISO 527
 65.0 MPa50 mm/min; ASTM D638
Elongation at Break 30 %50 mm/min; ISO 527
 80 %5 mm/min; ISO 527
 130 %50 mm/min; ASTM D638
 140 %5 mm/min; ASTM D638
Elongation at Yield 3.4 %5 mm/min; ISO 527
 3.5 %50 mm/min; ISO 527
 3.7 %50 mm/min; ASTM D638
 3.8 %5 mm/min; ASTM D638
Tensile Modulus 3850 MPa1mm/min; ISO 527
 4000 MPa5 mm/min; ASTM D638
Flexural Yield Strength 94.0 MPa2 mm/min; ISO 178
 99.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3500 MPa2 mm/min; ISO 178
 3700 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 180 J/mASTM D256
 100 J/m
@Temperature -30.0 °C
ASTM D256
 120 J/m
@Temperature 0.000 °C
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 20.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 11.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 60.0 JASTM D3763
 60.0 J
@Temperature -20.0 °C
ASTM D3763
Impact Test 100 JMultiaxial Impact; ISO 6603
Taber Abrasion, mg/1000 Cycles 30CS-17, 1 kg; SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 52.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 63.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 81.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 121 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 125 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 101 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 133 °CRate B/50; ISO 306
 134 °CRate B/50; ASTM D1525
 135 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 250 - 265 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 265 °C
Zone 3 250 - 270 °C
Melt Temperature 255 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10854 / 244321

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.