MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt Lucanex 716 Active Metal Brazing
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Brazing Paste Blended with Ti for active metal brazing of ceramics.

Information provided by Lucas-Milhaupt, Inc.

Alloy compositions are for filler metal powder in Lucanex paste

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 325 Mesh325 MeshPowder
Viscosity 300000 - 400000 cP300000 - 400000 cPPaste
 
Thermal PropertiesMetricEnglishComments
Melting Point 779.4 - 796.1 °C1435 - 1465 °F
Solidus 779.4 °C1435 °FMelting Point
Liquidus 796.1 °C1465 °FFlow Point
 
Processing PropertiesMetricEnglishComments
Processing Temperature 899 - 954 °C1650 - 1750 °FBrazing Range
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 28 %28 %
Nickel, Ni 0.50 %0.50 %
Silver, Ag 71.5 %71.5 %
Titanium, Ti 2.0 - 10 %2.0 - 10 %
 
Descriptive Properties
% Filler Metal Powder79-81% by Weight
ColorLight Brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt Cerametil 716 Active Metal Brazing
Lucas-Milhaupt Lucanex 616 Active Metal Brazing
Lucas-Milhaupt Cerametil 721 Active Metal Brazing
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Indium Corp. Indalloy 215 Silver Solder Alloy

NLUCMI64 / 18131

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.