Physical Properties | Metric | English | Comments |
---|
Density | 8.78 g/cc | 0.317 lb/in³ |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell B | 75 | 75 |
Hardness, Rockwell 30T | 72 | 72 |
Tensile Strength, Ultimate | 505 MPa | 73200 psi |
| >= 203 MPa @Temperature 315 °C | >= 29400 psi @Temperature 599 °F |
| >= 219 MPa @Temperature 290 °C | >= 31800 psi @Temperature 554 °F |
| >= 235 MPa @Temperature 260 °C | >= 34100 psi @Temperature 500 °F |
| >= 253 MPa @Temperature 230 °C | >= 36700 psi @Temperature 446 °F |
| >= 266 MPa @Temperature 205 °C | >= 38600 psi @Temperature 401 °F |
| >= 276 MPa @Temperature 175 °C | >= 40000 psi @Temperature 347 °F |
| >= 289 MPa @Temperature 150 °C | >= 41900 psi @Temperature 302 °F |
| >= 300 MPa @Temperature 120 °C | >= 43500 psi @Temperature 248 °F |
| >= 313 MPa @Temperature 95.0 °C | >= 45400 psi @Temperature 203 °F |
| >= 324 MPa @Temperature 65.0 °C | >= 47000 psi @Temperature 149 °F |
| >= 341 MPa @Temperature 23.0 °C | >= 49500 psi @Temperature 73.4 °F |
Tensile Strength, Yield | 486 MPa @Strain 0.2 % | 70500 psi @Strain 0.2 % |
| >= 116 MPa @Strain 0.2 %, Temperature 315 °C | >= 16800 psi @Strain 0.2 %, Temperature 599 °F |
| >= 123 MPa @Strain 0.2 %, Temperature 290 °C | >= 17800 psi @Strain 0.2 %, Temperature 554 °F |
| >= 127 MPa @Strain 0.2 %, Temperature 260 °C | >= 18400 psi @Strain 0.2 %, Temperature 500 °F |
| >= 131 MPa @Strain 0.2 %, Temperature 205 °C | >= 19000 psi @Strain 0.2 %, Temperature 401 °F |
| >= 131 MPa @Strain 0.2 %, Temperature 230 °C | >= 19000 psi @Strain 0.2 %, Temperature 446 °F |
| >= 135 MPa @Strain 0.2 %, Temperature 175 °C | >= 19600 psi @Strain 0.2 %, Temperature 347 °F |
| >= 139 MPa @Strain 0.2 %, Temperature 150 °C | >= 20200 psi @Strain 0.2 %, Temperature 302 °F |
| >= 144 MPa @Strain 0.2 %, Temperature 65.0 °C | >= 20900 psi @Strain 0.2 %, Temperature 149 °F |
| >= 144 MPa @Strain 0.2 %, Temperature 95.0 °C | >= 20900 psi @Strain 0.2 %, Temperature 203 °F |
| >= 144 MPa @Strain 0.2 %, Temperature 120 °C | >= 20900 psi @Strain 0.2 %, Temperature 248 °F |
| >= 150 MPa @Strain 0.2 %, Temperature 23.0 °C | >= 21800 psi @Strain 0.2 %, Temperature 73.4 °F |
Elongation at Break | 3.0 % | 3.0 % |
Creep Strength | >= 74.0 MPa @Temperature 315 °C | >= 10700 psi @Temperature 599 °F |
| >= 84.0 MPa @Temperature 290 °C | >= 12200 psi @Temperature 554 °F |
| >= 96.0 MPa @Temperature 260 °C | >= 13900 psi @Temperature 500 °F |
| >= 110 MPa @Temperature 230 °C | >= 16000 psi @Temperature 446 °F |
| >= 124 MPa @Temperature 205 °C | >= 18000 psi @Temperature 401 °F |
| >= 143 MPa @Temperature 175 °C | >= 20700 psi @Temperature 347 °F |
| >= 171 MPa @Temperature 150 °C | >= 24800 psi @Temperature 302 °F |
| >= 190 MPa @Temperature 120 °C | >= 27600 psi @Temperature 248 °F |
Rupture Strength | >= 47.0 MPa @Temperature 315 °C | >= 6820 psi @Temperature 599 °F |
| >= 65.0 MPa @Temperature 290 °C | >= 9430 psi @Temperature 554 °F |
| >= 82.0 MPa @Temperature 260 °C | >= 11900 psi @Temperature 500 °F |
| >= 105 MPa @Temperature 230 °C | >= 15200 psi @Temperature 446 °F |
| >= 125 MPa @Temperature 205 °C | >= 18100 psi @Temperature 401 °F |
| >= 148 MPa @Temperature 175 °C | >= 21500 psi @Temperature 347 °F |
| >= 171 MPa @Temperature 150 °C | >= 24800 psi @Temperature 302 °F |
Modulus of Elasticity | 121 GPa | 17500 ksi |
Poissons Ratio | 0.33 | 0.33 |
Fatigue Strength | 148 MPa @# of Cycles 1.00e+8 | 21500 psi @# of Cycles 1.00e+8 |
Machinability | 20 % | 20 % |
Forgeability | 65 % | 65 % |
Shear Modulus | 45.5 GPa | 6600 ksi |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 0.00000266 ohm-cm @Temperature 20.0 °C | 0.00000266 ohm-cm @Temperature 68.0 °F |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 16.3 µm/m-°C @Temperature 20.0 - 300 °C | 9.06 µin/in-°F @Temperature 68.0 - 572 °F |
Specific Heat Capacity | 0.385 J/g-°C | 0.0920 BTU/lb-°F |
Thermal Conductivity | 260 W/m-K @Temperature 20.0 °C | 1800 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
Melting Point | 1080 - 1090 °C | 1980 - 1990 °F |
Solidus | 1080 °C | 1980 °F |
Liquidus | 1090 °C | 1990 °F |
Annealing Point | 371 - 649 °C | 700 - 1200 °F |
|
Component Elements Properties | Metric | English | Comments |
---|
Copper, Cu | 97.5 % | 97.5 % |
Iron, Fe | 2.1 - 2.6 % | 2.1 - 2.6 % |
Lead, Pb | <= 0.030 % | <= 0.030 % |
Other, total | <= 0.15 % | <= 0.15 % |
Phosphorus, P | 0.015 - 0.15 % | 0.015 - 0.15 % |
Tin, Sn | <= 0.030 % | <= 0.030 % |
Zinc, Zn | 0.050 - 0.20 % | 0.050 - 0.20 % |